STRUKTOL® ZINC STEARATE
Subcategory: Additive/Filler for Polymer
Close Analogs: FDA Status: 175.105; 175.300; 176.170; 176.180; 176.200; 177.1460; 177.1900; 177.2410; 177.2600; 178.2010; 178.3910; 182.8994
Material Notes:
STRUKTOL® Zinc Stearate is one of the most widely used additives in the plastics field. It serves primarily as a lubricant, but also as a densifying agent and a partitioning agent. It is used extensively in color concentrates as a dispersion aid. It is used to improve processing of the styrenics and polyesters, and to a lesser extent with the olefins. In rubber applications, it functions as an elastomer processing aid and release agent.
| Available Properties |
- Additive Loading
- Particle Mesh Size
- Ash
- Melting Point
- Dropping Point
- Moisture Content
- Appearance
- Free Fatty Acid (%, max)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,