STRUKTOL® ZINC STEARATE CM
Subcategory: Additive/Filler for Polymer
Close Analogs: FDA Status: 175.105; 175.300; 176.170; 176.180; 176.200; 177.1460; 177.1900; 177.2410; 177.2600; 178.2010; 178.3910; 182.8994
Material Notes: A clear melt zinc stearate, is manufactured from high quality stearic acid in a tightly controlled production operation that guarantees product uniformity.STRUKTOL® Zinc Stearate CM, a clear melt zinc stearate, is manufactured from high quality stearic acid
in a tightly controlled production operation that guarantees product uniformity.
| Available Properties |
- Bulk Density
- Additive Loading
- Ash
- Dropping Point
- Moisture Content
- Shelf Life
- Appearance
- Free Fatty Acid (%, max)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|