STRUKTOL® V-PEAS Processing Additive

 

Subcategory: Additive/Filler for Polymer

Close Analogs: FDA Status: 178.369

Material Notes:
Polymeric complex ester of saturated fatty acids.

Typical Applications: STRUKTOL® V-PEAS is a very compatible complex ester lubricant. It has noted performance in clear–calendared sheet. It also has application in clear extrusion, blow bolding and injection molding formulations.

Features: STRUKTOL® V-PEAS is a very effective lubricant, albeit external, which has no negative impact on clarity in extrusion, calendaring, or injection molding. STRUKTOL® V-PEAS is noted to have ideal characteristics for calendared sheet where clarity is critical and where lower cost in performance is needed to replace montanic esters.

Available Properties
  • Specific Gravity
  • Additive Loading
  • Dropping Point
  • Shelf Life
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。