CARSTAB® DLTDP Thioester Antioxidant
Subcategory: Additive/Filler for Polymer
Close Analogs: FDA Status: 175.3
Key Words: C30H58O4S
Material Notes: Thioester synergist that is particularly effective as a long term heat aging stabilizer when used in conjunction with primary antioxidants.- CARSTAB DLTDP is especially recommended to protect high density polyethylene and ABS from oxidation in high temperature applications.
- CARSTAB DLTDP is also very effective in polypropylene and other polymers.
- For applications requiring superior heat stability, a combination of a hindered phenolic antioxidant and CARSTAB DLTDP should be used. It has been found that a combination of three parts of CARSTAB DLTDP is one part of hindered phenolic antioxidant often provides optimum performance. Typical use levels are 0.15% of CARSTAB DLTDP and 0.05% of phenolic antioxidant. It is recommended that specific end use formulations be optimized with regard to thioester synergist ratio and use level.
| Available Properties |
- Specific Gravity
- Additive Loading
- Molecular Weight
- Acid Value
- Melting Point
- Transmission, Visible
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|