CARSTAB® DSTDP Thioester Antioxidant

 

Subcategory: Additive/Filler for Polymer

Close Analogs: FDA Status: 175.105; 175.300

Key Words: C42H82O4S

Material Notes:

  1. CARSTAB DSTDP is especially recommended to protect polypropylene from oxidation in high temperature applications.
  2. CARSTAB DSTDP is also very effective in polyethylene and other polymers.
  3. For applications requiring superior heat stability, a combination of a hindered phenolic antioxidant and CARSTAB DSTDP should be used. It has been found that a combination of three parts of CARSTAB DSTDP is one part of hindered phenolic antioxidant often provides optimum performance. Typical use levels are 0.15% of CARSTAB DSTDP and 0.05% of phenolic antioxidant. It is recommended that specific end use formulations be optimized with regard to thioester synergist ratio and use level.

Available Properties
  • Specific Gravity
  • Additive Loading
  • Molecular Weight
  • Acid Value
  • Melting Point
  • Transmission, Visible
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。