STRUKTOL® TPW 709 Processing Additive
Subcategory: Additive/Filler for Polymer
Material Notes: A unique proprietary blend of non-metal internal/external processing aids.Applications: STRUKTOL® TPW 709 has shown excellent results in producing extruded polymer/wood composites with or without coupling agents at a lower dosage than other lubricants on the market. Information provided by Struktol
| Available Properties |
- Specific Gravity
- Additive Loading
- Dropping Point
- Shelf Life
- Appearance
|
|
|
|