STRUKTOL® TPW 609 Processing Additive
Subcategory: Additive/Filler for Polymer
Material Notes: Blend of complex, modified fatty acid ester.Applications: STRUKTOL® TPW 609 has shown excellent results in producing extruded polymer / wood composites with or without coupling agents at a lower dosage than other lubricants on the market. STRUKTOL® TPW 609 offers very good mixing, improved filler dispersion and improved extrusion rates. Information provided by Struktol
| Available Properties |
- Specific Gravity
- Additive Loading
- Dropping Point
- Shelf Life
- Appearance
|
|
|
|