STRUKTOL® V-HCS Co-Stabilizing Processing Additive
Subcategory: Additive/Filler for Polymer
Material Notes: Blend fatty acid derived and functional inorganic materials.Applications: STRUKTOL® V-HCS is recommended for us with recycled rigid PVC where additional stabilization and lubrication is needed to reduce yellowing, burning and sticking in extrusion, injection molding and calendering. It is especially useful in allowing higher loadings of PVC regrind (post industrial or post consumer) in virgin formulations. It also allows for longer production runs between shutdowns due to degradation. Information provided by Struktol
| Available Properties |
- Specific Gravity
- Additive Loading
- Melting Point
- Shelf Life
- Appearance
|
|
|
|