STRUKTOL® POLYDIS 3615 Elastomer modified epoxy prepolymer
Subcategory: Epoxy; Additive/Filler for Polymer
Material Notes:
Applications: STRUKTOL VP 3615 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength. Contrary to PD 3614 the Tg decrease less, but fracture toughness is on the same level. Information provided by Struktol