STRUKTOL® POLYDIS 3622 Elastomer modified epoxy prepolymer
Subcategory: Epoxy; Additive/Filler for Polymer
Material Notes:
Applications: STRUKTOL VP 3622 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength. Information provided by Struktol
| Available Properties |
- Density
- Viscosity
- Acid Value
- Shelf Life
- Appearance
- Elastomer Content %
- Epoxy Equivalent Weight (g/Eq)
- Resin-base of the prepolymer
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|