STRUKTOL® VP 3643 Optimized elastomer-modified epoxy prepolymer
Subcategory: Epoxy; Additive/Filler for Polymer
Material Notes: Optimized elastomer-modified epoxy prepolymer for the flexibilisation of epoxy resin systemsApplications: STRUKTOL VP 3643 is used when conventional epoxy systems do not meet the requirements regarding impact resistance, bending resistance or low temperature flexibility. Information provided by Struktol
| Available Properties |
- Density
- Viscosity
- Acid Value
- Shelf Life
- Appearance
- Elastomer Content %
- Epoxy Equivalent Weight (g/Eq)
- Resin-base of the prepolymer
|
|
|
|