STRUKTOL® STRUKSILON 8018 Silicone Stabiliser for PU-Microcellular Foam
Subcategory: Additive/Filler for Polymer
Material Notes: STRUKSILON 8018 is used as a silicone stabilizer for the production of polyurethane microcellular foam. It is especially recommended for shoe sole formulations based on polyester and blends of polyether/polyester polyols.Applications: Information provided by Struktol
| Available Properties |
- Density
- Viscosity
- Flash Point
- Refractive Index
- Shelf Life
- Appearance
- Turbidity Point °C
|
|
|
|