STRUKTOL® STRUKSILON 8030 Silicone Stabiliser for PU-Rigid Foam
Subcategory: Additive/Filler for Polymer
Material Notes: STRUKSILON 8030 is a universal stabilizer for the production of polyurethane rigid foams. Due to its excellent flow properties and the very good insulation values that can be achieved STRUKSILON 8030 is especially recommended for 141 b blown formulation for appliance applications, pipe insulation and the production of PUR panels. Good results may also be achieved, when used in n-,i- or cyclopentane blown systems. For these formulations the system compatibility should be checked.Applications: Information provided by Struktol
| Available Properties |
- Density
- Viscosity
- Flash Point
- Refractive Index
- Appearance
- Turbidity Point °C
|
|
|
|
| Property Data |