STRUKTOL® STRUKSILON 8118 Silicone Stabiliser for PU Foam
Subcategory: Additive/Filler for Polymer
Material Notes: STRUKSILON 8118 is a silicone stabilizer for liquid-CO2 of medium potency for the production of flexible polyurethane slabstock foam based on polyether polyols.Applications: STRUKSILON 8118 was especially developed for the production of liquid-CO2 blown PU slabstock foam. Additionally, STRUKSION 8118 can be used in conventional PU slabstock foam blown with water or physical blowing agents and works in nearly all known flexible PU slabstock foam applications. Information provided by Struktol
| Available Properties |
- Density
- Viscosity
- Flash Point
- Shelf Life
- Appearance
- Turbidity Point °C
|
|
|
|