Süd-Chemie Nanofil® 5 Flame Retardant
Subcategory: Additive/Filler for Polymer
Key Words: Sud-Chemie
Material Notes: Standard grades for inorganic flame retardant cable formulations with good pre-dispersibility.Application: - PE/EVA
- Grafted PP Cable formulation
- Automotive
- Technical Parts
Improves: Abrasion/Scratch Resistance
| Available Properties |
- Additive Loading
- Melt Flow
- Elongation at Break
- Flammability, UL94
- Type
|
|
|
|