Sunoco Chemical FT200WV Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Good Mold Release, Nucleated, Excellent Rigidity and Hardness
Material Notes: Market Segment: Caps and Closures Suggested Uses Include Housewares, Caps and Closures, Fast-Cycle Injection Molding Information provided by Sunoco Chemicals. Available in Canada.
| Available Properties |
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Process
|
|
|
|