Sunoco Chemical TI4500WV2 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Key Words: High Melt Flow, Nucleated, Excellent Mold Release, Antistatic
Material Notes: Market Segment: Consumer Products Suggested Uses Include Housewares, Large Part Injection Molding, Thin-Walled Injection Molding Information provided by Sunoco Chemicals.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|