Sunoco Chemical TI4700P2 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Key Words: Very High Flexural Modulus
Material Notes: Market Segment: Consumer Products; Compounding Suggested Uses Include Compounding, Automotive Interior Trim, Intricately Designed Parts, Thin-Walled Parts, Dairy Containers, Building and Construction Information provided by Sunoco Chemicals.