Sunoco Chemical TI6120Q4 Polypropylene High Impact Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Extra High Izod Impact, Superior Low Temperature Drop Impact
Material Notes: Market Segment: Compounding Suggested Uses Include Automotive, Compounding Information provided by Sunoco Chemicals. Available in Canada.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact Test
- Izod Impact, Notched
- Process
|
|
|
|