Supreme Petrochem SC 203EL General Purpose Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Characteristics- Medium flow grade with good mechanical properties
- Improves productivity due to good balance of flow, heat and mold release properties
ProcessingApplications- Audio cassettes housing and covers
- Medical applications like disposable infusion trays, screw vials etc.
- Crystal wares, mugs, trays, bowls, pen stands, fruit bowls, service trays etc.
Material Status: Commercial : Active Agency Ratings: FDA 21 CFR 177.1640, UL file E185934 Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|