Supreme Petrochem SH 400 M High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: CharacteristicsProcessingApplications- Air conditioner and cooler grills, refrigerator components
- Toys, use and throw camera, household articles
- Ball pen barrels, novelties, stationary items
- Washing machine & small appliances
Material Status: Commercial : Active Agency Ratings: FDA 21 CFR 177.1640 Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,