Supreme Petrochem SP 566 Flame Retardant Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Characteristics- Good flow and toughness
- Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU
- Available in any color
ProcessingApplications- Large size T.V. Cabinets
- Electrical appliance parts, business machines
- Sheets for mass transit furnishing etc.
Material Status: Commercial : Active Agency Ratings: UL 94 file E 185934 Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
- Melt Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|