Supreme Petrochem SC 6501 Toughened Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Characteristics- Excellent melt strength
- Extremely tough
- Easy printability
- Easy miscibility with most grades of polystyrene
Processing- Extrusion
- Thermoforming
- Injection Molding
Applications- Impact modifier for HIPS for industrial thermoforming
- Toys, appliances requiring very high toughness
Material Status: Commercial : Active Agency Ratings: FDA 21 CFR 177.1640 Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|