Supreme Petrochem SP 6425 9885 Abrasion Resistant Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Characteristics- Low friction, impact polystyrene to provide wear resistance and static charge dissipation
- Excellent gloss & molded appearance and weld line miscibility
- Easy flowing grade with good impact resistance
ProcessingApplications- High speed molding of thin walled 3.5" Microfloppy diskettes shells and other magnetic storage devices
Material Status: Commercial : Active Agency Ratings: Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Surface Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|