Supreme Petrochem SP 8001 High Gloss, ESCR High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Characteristics- Very high toughness
- Excellent ESCR properties against common food chemicals
- High gloss & heat resistance
ProcessingApplications- Fatty food containers
- Co-extrusion for refrigerator liners
- Dairy containers
- Industrial formed containers
Material Status: Commercial : Active Agency Ratings: FDA 21 CFR 177.1640 Information provided by Supreme Petrochem LTD
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|