Sylvin Technologies, Inc. 500 PVC Wire/Cable Compound
Subcategory: Vinyl; Thermoplastic
Material Notes: Sylvin 500 is a vinyl compound formulated for insulating and jacketing application, especially underground feeder wire. This compound has a Underwriters Laboratories yellow card for TW type wire and for 300 hour Sunlight Resistance.Information provided by Sylvin Technologies Inc.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Brittleness Temperature
- Flammability, UL94
- Oxygen Index
- Processing Temperature
|
|
|
|