Teijin Panlite LN-2250Y Flame Resistant, Translucent Polycarbonate Resin
Subcategory: Polycarbonate; Thermoplastic
Material Notes: Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications: Electric, electronic and business machine components that need flame retardancy.Information provided by Teijin Chemicals Ltd.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Refractive Index
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|