Teijin Panlite LS-2250 Friction and Abrasion Resistant Polycarbonate Resin
Subcategory: Polycarbonate; Thermoplastic
Material Notes: It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excellent properties of polycarbonate resin. Also provided are those reinforced with GF and CF.Applications: Mechanical, electric and electronic components that need abrasion and friction resistance.Information provided by Teijin Chemicals Ltd.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|