Teknor APEX® 3210-65 Polyvinyl Chloride, Flexible
Subcategory: Vinyl; Thermoplastic
Material Notes:
Material Status-Commercial: Active Availability-North America Test Standards Available-ASTM Features-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, General Purpose, Medical Applications, Valves/Valve Parts, Wire & Cable Applications Appearance-Natural, Opaque Forms-Pellets Processing Method-Injection Molding Information provided by Teknor Apex Company
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Break
- Brittleness Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|