Teknor APEX® 90-A472R-100-NT Polyvinyl Chloride, Flexible
Subcategory: Vinyl; Thermoplastic
Material Notes:
Material Status-Commercial: Active Availability-North America Test Standards Available-ASTM Uses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-Clear Forms-Pellets Processing Method-Injection MoldingInformation provided by Teknor Apex Company