Teknor Flexalloy® 9800-40 Polyvinyl Chloride Elastomer
Subcategory: Vinyl; Elastomer, TPE; Thermoplastic
Material Notes:
Material Status-Commercial: Active Availability-North America Test Standards Available-ASTM Features: Oil Resistant, Ultra High MW Uses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and Cable Applications, Seals Forms-Pellets Processing- ExtrusionInformation provided by Teknor Apex Company
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Brittleness Temperature
- Swell
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,