Solvay Solexis Algoflon® S 121 PTFE (Polytetrafluoroethylene)
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: Data provided by the manufacturer. Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Coefficient of Friction
- Coefficient of Friction, Static
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Thermal Conductivity
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|