Solvay Solexis Algoflon® E2 PTFE (Polytetrafluoroethylene)
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: Data provided by the manufacturer. Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Tensile Strength, Ultimate
- Elongation at Break
- Coefficient of Friction
- Coefficient of Friction, Static
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Thermal Conductivity
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|