Solvay Solexis Algoflon® 35CAR PTFE; Petroleum Coke and Graphite
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Key Words: Petroleum Coke; Graphite
Material Notes: Data provided by the manufacturer. 35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Coefficient of Friction
- Coefficient of Friction, Static
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|