Asahi Kasei Thermylene® P-20TC-1156 Chemically Coupled Polypropylene Compound, 20% Talc Filled
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|