Tipco - Tipcolite® THD 321 - Thermoset Phenolic Compound, Reinforced with Wood Flour & Cellulose, having Soft Flow & High Strength
Subcategory: Phenolic; Thermoset
Material Notes: Soft Flow Phenolic Compound, Reinforced with Wood Flour & Cellulose Applications: Switchgear, HRC Fuses Processing: Compression & Transfer Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Izod Impact, Unnotched (ISO)
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|