Tipco - Tipcolene® FPTC 60 - 60% Talc & Calcium Carbonate Reinforced Polypropylene Homopolymer Masterbatch
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: 60% Talc+Calcium Reinforced PP Homopolymer Applications: Furniture & Appliances Processing: Injection Molding Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
|
|
|
|