Tipco Tipcolene® SEB 300 - 30% Chemically Coupled Glass Fibers Reinforced Polypropylene Homopolymer Compound with High Heat Stability
Subcategory: Polypropylene; Thermoplastic
Material Notes: 30% Chemically Coupled Glass Reinforced PP Homopolymer Applications: General Purpose Processing: Injection Molding Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|