Tipco - Tipcolite® TPF 1119 - Latex Modified Thermoset Phenolic Resin having 26mm Norton Flow with 9% Hexamine
Subcategory: Phenolic; Thermoset
Material Notes: Latex Modified Phenolic Resin having 26mm Norton Flow, in Powder Form Applications: Automotive & Industrial Processing: Brakelining Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
| Available Properties |
- Spiral Flow
- Melting Point
|
|
|
|
| Property Data |