Tipco - Tipcolite® TPF 151 - Thermoset Phenolic Resin having 128 cps Viscosity containing 65% Solids
Subcategory: Phenolic; Thermoset
Material Notes: Phenolic Resin having 128 cps Viscosity, in Liquid Form Applications: Foundry & Hot Box Processing: Castings & Shells Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|
|