Tipco - Tipcolite® TPF 1514 - Thermoset Phenolic Resin having 230 cps Viscosity containing 59% Solids
Subcategory: Phenolic; Thermoset
Material Notes: Phenolic Resin having 230 cps Viscosity, in Liquid Form Applications: Textile, Paper Impregnation Processing: Hand Lay-up Information provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|
|