TITANPRO® PD855 Polypropylene homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9003-07-0
Material Notes: The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: Slit tape and monofilament for rope, twine, yarn and industrial fabrics. Advantages: - Outstanding process-ability.
- Maximum bubble stability for slit tape production by the tubular process.
- Good melt stability.
- Low color. Low taste and odor.
- No plate out problems on die lips or chill rolls.
- Good heat-aging stability in yarn and fabric.
Fabrication: - Equipment - general extrusion.
- Techniques - standard processing for tubular and flat die tapes.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|