TITANPRO® PD943 Polypropylene homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9003-07-0
Material Notes: The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: - Bags for hosiery, shirts and other textiles.
- Food packaging for fresh fruits and produce.
Advantages: - Good optical properties.
- Excellent stiffness.
- High slip development and good open-ability.
Fabrication: - Equipment - general water quench blown film machines.
- Techniques - standard processing. Extrusion and water bath conditions can be varied to obtain the desired optical and mechanical film properties
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|