TITANPRO® PM801 Polypropylene homopolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9003-07-0
Material Notes: Titanpro® PM801 is a clarified, high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: - Thin walled injection molding (TWIM) articles.
- Disposable containers and lids, party plates, pen barrels, document case, compounding purposes.
Advantages: - Low molded in stress.
- Good clarity.
- Good balance of stiffness and impact strength.
- Short cycle time.
- Microwaveable for food reheating purposes.
Fabrication: - Equipment - ram or screw injection machines.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|