TITANPRO® SM256 Polypropylene random copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9010-79-1
Material Notes: Titanpro® SM256 is designed for high clarity articles. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: - Injection and extrusion blow molding containers.
- Extruded sheet for thermoformed containers and lids, etc.
- Multilayer co-extruded structures and sheet.
- Injection molded articles requiring high toughness.
Advantages: - Superior clarity.
- Low odor and taste.
- Good rigidity and impact resistance.
- Process versatility.
- Hot fillable.
Fabrication: - Equipment - general injection, extrusion blow molding, sheet extrusion and thermoforming machines.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|