TITANPRO® SM511C Polypropylene random copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Titanpro® SM511C was created for extrusion coating on BOPP films.Applications: - Heat sealable layer.
- Quality packaging application.
Advantages: - Low heat sealing temperature.
- Good bond strength.
- Excellent gloss and clarity.
- Good process-ability.
Fabrication: - Equipment - general extrusion coating line.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|