TITANPRO® SM668 Polypropylene random copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9010-79-1
Material Notes: Titanpro® SM668 is a clarified grade designed for high transparency articles. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: - High clarity oriented PP bottles for hot filled applications, moisture sensitive packaging, baby feed bottles, toiletries and detergent packaging, etc.
- High transparent thin walled containers, storage containers, large articles, house-wares.
Advantages: - Excellent clarity.
- Good balance of rigidity and impact resistance.
- Excellent moisture barrier.
- Suitable for hot filling and thin walled products.
Fabrication: - Equipment - injection stretch blow molding (ISBM) machine, injection molding machine.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|