TITANPRO® SM669 Polypropylene random copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Titanpro® SM669 is a clarified grade designed for high transparency articles.Applications: DVD casing, high transparent thin walled containers, storage containers. Advantages: - Excellent clarity.
- Good balance of rigidity and impact resistance.
- Good dimensional stability.
Fabrication: - Equipment - injection molding machine.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|