TITANPRO® SM850 Polypropylene impact copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: CAS# 9010-79-1
Material Notes: Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: Automotive parts, appliances, house-wares, washing machine tub and parts, large flat trays, thin walled containers. Advantages: - Easy processing, permitting wider latitude in design.
- Good toughness at low temperature.
- Good surface finish and color.
- Low molded in stress.
- Excellent heat stability.
Fabrication: - Equipment - ram or screw injection machines.
- Techniques - standard processing.
Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- Water Absorption
- Base Resin Melt Index
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Dart Drop, Total Energy
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|