TITANEX® LI2516 Linear low density polyethylene resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys. Advantages: Excellent stress crack resistance, toughness and gloss, superior molding properties, low odor. Information provided by Titan Chemicals
| Available Properties |
- Base Resin Density
- ESCR 100% Igepal®
- Base Resin Melt Index
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- 1% Secant Modulus
- Vicat Softening Point
- Brittleness Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|